Mechanical Properties Metric English Comments
Flexural Yield Strength 49.0 - 151 MPa
7110 - 21900 psi
Average value: 74.3 MPa Grade Count:21
Overview of materials for ABS/Polyester Alloy
This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat..