Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 12.8 - 162 MPa | 1850 - 23500 psi | Average value: 119 MPa Grade Count:40 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Flexural Yield Strength | 49.6 - 162 MPa | 7200 - 23500 psi | Average value: 89.6 MPa Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is m.. |