Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 237 MPa | 34400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36 PPS LNP* LUBRICOMP* OCP36 is a compound based on Polyphenylene Sulfide resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Wear Resistant, Bearing Grade, Electr.. |
|||
Flexural Yield Strength | 237 MPa | 34400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON REL33 PA 66 LNP STAT-KON* REL33 is a compound based on Nylon 66 resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Flexural Yield Strength | 237 MPa | 34400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Stat-kon RE003 PA 66 (Europe-Africa-Middle East) LNP* Stat-kon* RE003 is a compound based on Nylon 66 resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |