Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 54.0 - 167 MPa | 7830 - 24200 psi | Average value: 111 MPa Grade Count:43 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |