Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 170 MPa | 24600 psi | ASTM D790 |
Westlake Plastics Tefzel® 2181 ETFE Products made from Tefzel® HT-2181 resin are suitable for a variety of processes and demanding end uses. They are mechanically tough and offer an excellent balance of properties. These products p.. |
|||
Flexural Yield Strength | 169.6 MPa | 24600 psi | ASTM D790 |
Plenco 50240 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black.. |