Polymer Property : Flexural Yield Strength = 25050 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 172.7 MPa
25050 psi
ASTM D790
Plenco 50240 PET, Pellet, Injection Molded, Green  (discontinued **)
PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black..