Mechanical Properties Metric English Comments
Flexural Yield Strength 2600 MPa
377000 psi
57 HRC. Four point bend testing. 5 mm ø. 5mm/min. Austenitizing temperature: 990-1180°C, Tempering: 3X1 h at 560°C
Assab Steels ASP 23 Cold Work Steel
ASP 23 is a chromium-molybdenum-tungsten-vanadium alloyed high speed steel which is characterized by:High wear resistance (abrasive profile)High compressive strengthVery good through-hardening prope..