Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 187.2 MPa | 27150 psi | ASTM D790 |
Plenco 50335 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 50335 is an engineering grade glass reinforced polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white, natural, and black.Inform.. |