Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 281 MPa | 40800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RCL34 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RCL34 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Yield Strength | 281 MPa | 40800 psi | Flexural elongation is 2.1%; ASTM D790 |
Toyobo TS501 PPS, 50% Glass Fiber Reinforced Key Feature: High stiffnessHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excellent physical, e.. |
|||
Flexural Yield Strength | 281 MPa @Thickness 3.20 mm |
40800 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUXY KS G55 Amorphous PA6 Description: Injection Molding, Amorphous PA6, High Modulus, High Impact, Low WarpageApplication: Electric/Electronic Components (LCD Bracket)Information provided by LG Chemical |