Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 297 MPa | 43100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP VERTON RX00327 PA 66 LNP* VERTON* RX00327 is a compound based on Nylon 66 resin containing proprietary fillers. Added feature of this material is: Structural. |