Polymer Property : Flexural Yield Strength = 29810 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 205.5 MPa
29810 psi
ASTM D790
Plenco 51030 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 51030 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for good physical strength. It is UL listed.Information supplied by PlencoPlenco discontinued..