Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 301 MPa | 43700 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP LC006 PEEK (Europe-Africa-Middle East) LNP* THERMOCOMP* LC006 is a compound based on Polyetheretherketone containing Carbon Fiber. Added features include: Electrically Conductive. |