Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 103 - 324 MPa | 15000 - 47000 psi | Average value: 172 MPa Grade Count:10 |
Overview of materials for Nylon 66, Mineral Filled, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, NCG Fiber Filled". Each property range of values reported is minimum and maxim.. |