Polymer Property : Flexural Yield Strength = 33.19 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 33.19 MPa
4814 psi
ASTM D790
KKPC Kuhmo HI 425TVG High Flow/High Heat Resistant HIPS
Key features: High-impact, High-fluidity Common Uses: TV cover (gas injection).HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between im..