Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 117 - 228 MPa | 17000 - 33100 psi | Average value: 154 MPa Grade Count:16 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |