Mechanical Properties Metric English Comments
Flexural Yield Strength 65.0 - 234 MPa
9430 - 34000 psi
Average value: 146 MPa Grade Count:71
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..
Flexural Yield Strength 95.0 - 234 MPa
13800 - 34000 psi
Average value: 148 MPa Grade Count:31
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max..