Mechanical Properties Metric English Comments
Flexural Yield Strength 239 MPa
34700 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXP PPA (Europe-Africa-Middle East)
LNP* LUBRICOMP* UFL36SXP is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated, Heat Stabilized.
Flexural Yield Strength 239 MPa
34700 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP QF007 PA 6/10
LNP* THERMOCOMP* QF007 is a compound based on Nylon 6/10 resin containing 35% Glass Fiber.