Flexural Yield Strength 293 MPa
42500 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP VC006 SUPER TOUGH NYLON
LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon resin containing 30% Carbon Fiber. Added features of this material include: High Impact, Electrically Conductive.
Flexural Yield Strength 293 MPa
42500 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOTUF VC006 Super Tough PA 6/6
LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon 6/6 resin containing Carbon Fiber. Added features of this material include: High Impact.