Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 294 MPa | 42600 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha.. |
|||
Flexural Yield Strength | 294 MPa | 42600 psi | Conditioned; ASTM D790 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0... |
|||
Flexural Yield Strength | 294 MPa | 42600 psi | ASTM D790 |
Plenco 50045 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 50045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is UL listed and available in white, natural, and black.Information s.. |