Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 30.4 MPa @Thickness 6.40 mm |
4410 psi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL EI5002 PP Description: Injection Molding, PP, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 9002-88-4Information provided by LG Chemical |
|||
Flexural Yield Strength | 30.4 MPa | 4410 psi | ASTM D790 |
Eastman Tenite 285A3R30018 Butyrate Natural, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |