Polymer Property : Flexural Yield Strength = 50.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 50.3 MPa
7300 psi
ASTM D790
Ineos ABS Lustran® 743 General Purpose, High-Impact  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionLANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La..
Flexural Yield Strength 50.3 MPa
7300 psi
ASTM D790
Techmer ES HiFill® ABS GB10 10% Glass Bead Filler
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc.
Flexural Yield Strength 50.3 MPa
7300 psi
ASTM D790
Techmer ES HiFill® ABS GB15 15% Glass Bead Filler
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc.