Polymer Property : Flexural Yield Strength = 52100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 359 MPa
52100 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP 9X06030 PA 46 (Europe-Africa-Middle East)
LNP* LUBRICOMP* 9X06030 is a compound based on PA46 resin containing PTFE and Carbon Fiber. Added features include: Internally Lubricated, Heat Stabilized.
Flexural Yield Strength 359 MPa
52100 psi
ASTM D790
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA), 45% Glass Fiber
Amodel® AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e..
Flexural Yield Strength 359 MPa
52100 psi
ASTM D790
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee..