Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 36.5 MPa | 5290 psi | ASTM D790 |
Tipco Tipcolene® FPT 10 PPC - 10% Talc Reinforced Polypropylene Copolymer Compound 10% Talc Reinforced PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Yield Strength | 36.5 MPa | 5290 psi | ASTM D790 |
Tipco Tipcolene® FPC 30 PPC - 30% Calcium Carbonate Reinforced Polypropylene Copolymer 30% Calcium Carbonate Filled PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |