Polymer Property : Flexural Yield Strength = 5580 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 38.5 MPa
5580 psi
ASTM D790
Tipco Tipcolene® HR 8240 - 10% Talc/Mineral Reinforced Impact Modified Polypropylene Copolymer, High Stiffness
10% Mineral Reinforced, High Stiffness, Impact Modified PP CopolymerApplications: Automotive ExteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., I..