Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 56.5 MPa | 8200 psi | ASTM D790 |
Ravago Manufacturing Americas Hylac® HF224 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Yield Strength | 56.5 MPa | 8200 psi | ASTM D790 |
PlastxWorld DAICEL STYROL® SK50H HIPS Flame retarded HIPSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |