Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Yield Strength = 56.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 56.9 MPa

@Thickness 3.20 mm
8250 psi

@Thickness 0.126 in
15 mm/min; ASTM D790
LG Chemical RX710 ABS, High Impact, Chemical Resistance to HCFC
Feature: Injection Molding, Chemical Resistance to HCFC, High ImpactApplication: Refrigerator Dispensor & HomebarCAS No. 9003-56-9Information provided by LG Chemical
Flexural Yield Strength 56.9 MPa

@Thickness 3.20 mm
8250 psi

@Thickness 0.126 in
15 mm/min; ASTM D790
LG Chemical SH610S ABS, Excellent Surface, High Impact
Feature: Extrusion Molding, Excellent Surface, High ImpactApplication: Bag, miscellaneousCAS No. 9003-56-9Information provided by LG Chemical
Flexural Yield Strength 56.9 MPa
8250 psi
ASTM-D790
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned)
Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce..
Flexural Yield Strength 56.9 MPa

@Thickness 6.40 mm
8250 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron AN-450 Flame Retardant ABS Grade
Information provided by Bhansali
Flexural Yield Strength 56.9 MPa

@Thickness 6.40 mm
8250 psi

@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron AN450M Flame Retardant ABS
Flame Retardant- V0 at 3.0mm (UL 94 certified)Information provided by Bhansali
Flexural Yield Strength 56.9 MPa

@Thickness 6.40 mm
8250 psi

@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron SE32H Extrusion ABS
Very High Impact, Better Flow and Sheet/Pipe/Profile applicationInformation provided by Bhansali
Flexural Yield Strength 56.9 MPa

@Thickness 6.40 mm
8250 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron AN-450 EVM Flame Retardant ABS Grade
Information provided by Bhansali
Flexural Yield Strength 56.9 MPa

@Thickness 6.40 mm
8250 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron AN-450 Flame Retardant ABS Grade
Information provided by Bhansali
Flexural Yield Strength 56.9 MPa

@Thickness 6.40 mm
8250 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron AN-450 EVM Flame Retardant ABS Grade
Information provided by Bhansali
Flexural Yield Strength 56.9 MPa

@Thickness 6.40 mm
8250 psi

@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron AN450M Flame Retardant ABS
Flame Retardant- V0 at 3.0mm (UL 94 certified)Information provided by Bhansali
Flexural Yield Strength 56.9 MPa

@Thickness 6.40 mm
8250 psi

@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron SE32H Extrusion ABS
Very High Impact, Better Flow and Sheet/Pipe/Profile applicationInformation provided by Bhansali