Mechanical Properties Metric English Comments
Flexural Yield Strength 0.392 MPa
56.9 psi
30g/L; KS M 3808
LG Chemical B160 EPS, Non-Flame Retardant
Feature: Expendable Polystyrene, Non-Flame RetardantApplication: Package, Fruit/Fish Box, Floats, Pad, Ice BoxCAS No. 9003-53-6 and 109-66-0Information provided by LG Chemical