Mechanical Properties Metric English Comments
Flexural Yield Strength 57.23 MPa
8301 psi
Abatron AboCast 8-19/Abocure 8-19 Epoxy  (discontinued **)
2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/32.00 ratio (pbw); Gel time, 100 g (3.5 oz.): 120 minutes; cures in 2 weeks at 25°C (77°F).Applications: solventless c..