Polymer Property : Flexural Yield Strength = 6240 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 29.8 - 43.0 MPa
4320 - 6240 psi
Average value: 34.5 MPa Grade Count:6
Overview of materials for High Density Polyethylene (HDPE), Wood Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Wood Filled". Each property range of values reported is minimum and ma..