Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 7.85 MPa | 1140 psi | ASTM D790 |
Samyang Triel® 5500 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5500 is an extrusion grade.Information provided by Samyang. |