Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 48.4 MPa | 7020 psi | ASTM D790 |
Spartech Royalite R632M Carbon Black Filled ABS/PVC Resin Data provided by the manufacturer. This static-conductive material is UL®-listed and meets minimum static-decay requirements outlined in MIL-B-1705B and NFPA Code 56A specifications. |