Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 71.6 MPa @Thickness 3.20 mm |
10400 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical BM662 ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical.. |
|||
Flexural Yield Strength | 71.6 MPa @Thickness 3.20 mm |
10400 psi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical Lupox® GP1000SB PBT Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Flexural Yield Strength | 71.6 MPa @Thickness 3.20 mm |
10400 psi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical Lupox® GP1006FD PBT Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica.. |
|||
Flexural Yield Strength | 71.6 MPa @Thickness 3.20 mm |
10400 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY MP5000AM PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Metal PlatingApplication: Automotive (Exterior), E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 71.6 MPa @Thickness 3.20 mm |
10400 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR419 ABS, Heat Resistance, Chemical Resistance Feature: Injection Molding, Heat Resistance, Chemical ResistanceApplication: Automotives Interior Housing (Ventgrille Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provide.. |
|||
Flexural Yield Strength | 71.6 MPa @Thickness 3.20 mm |
10400 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR474F ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Exterior Housing (Lamp Housing Etc)CAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical |
|||
Flexural Yield Strength | 71.6 MPa @Thickness 3.20 mm |
10400 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR404HJ ABS, Heat Resistance, Curl Fit Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chemica.. |
|||
Flexural Yield Strength | 71.6 MPa @Thickness 6.40 mm |
10400 psi @Thickness 0.252 in |
ASTM D790 |
Bhansali Engineering Abstron IM-21 ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Flexural Yield Strength | 71.6 MPa @Thickness 6.40 mm |
10400 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron KU650NH ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Flexural Yield Strength | 71.6 MPa @Thickness 6.40 mm |
10400 psi @Thickness 0.252 in |
ASTM D790 |
Bhansali Engineering Abstron IM-21 ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Flexural Yield Strength | 71.6 MPa @Thickness 6.40 mm |
10400 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron KU660 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Flexural Yield Strength | 71.6 MPa @Thickness 6.40 mm |
10400 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron KU650NH ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Flexural Yield Strength | 71.6 MPa @Thickness 6.40 mm |
10400 psi @Thickness 0.252 in |
5 mm/min; ASTM D790 |
Bhansali Engineering Abstron KU660 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |