Mechanical Properties Metric English Comments
Flexural Yield Strength 49.0 MPa
7100 psi
ASTM D790
Spartech Royalstatâ„¢ R63 ABS/PVC Static Control Sheet
Description: Static Control SheetInformation provided by Spartech.
Flexural Yield Strength 49.0 MPa
7100 psi
ASTM D790
Clariant Renol CAB1000 Cellulose Acetate Butyrate
Data provided by Clariant Masterbatches
Flexural Yield Strength 49.0 MPa
7100 psi
ASTM D790
PlastxWorld DAICEL STYROL® GW30 HIPS
UV stable flame retarded HIPSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.