Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 72.6 MPa
10500 psi
15 mm/min. ASTM D790
Techno Polymer Techno ABS LM100 Transparent
Excellent shock resistance, rigidity, and processability.Applications: Appliance parts, office and computer equipment, machine parts, and tool handles.
Flexural Yield Strength 72.6 MPa

@Thickness 3.20 mm
10500 psi

@Thickness 0.126 in
15mm/min; ASTM D790
LG Chemical LI970 Co-Extrusion ASA
Description: Good Weatherability, Scratch ResistanceApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical
Flexural Yield Strength 72.6 MPa

@Thickness 3.20 mm
10500 psi

@Thickness 0.126 in
15 mm/min; ASTM D790
LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC
Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Flexural Yield Strength 72.6 MPa

@Thickness 6.40 mm
10500 psi

@Thickness 0.252 in
15 mm/min; ASTM D790
LG Chemical TR557 MABS, High Transparency, High Impact
Feature: Injection Molding, High Transparency, High ImpactApplication: Electric/Electronic Applications, Copier, Printer etc.CAS No. 9011-14–7 and 9003-56-9Information provided by LG Chemical
Flexural Yield Strength 72.6 MPa
10500 psi
ASTM D790
IRPC Polimaxx Polene 2511HX GA5 Polypropylene Compound
CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 25% GLASS FIBRE REINFORCED VERY HIGH IMPACT STRENGTH, HIGH MECHANICAL STRENGTH, LOW SHRINKAGE, HIGH STIFFNESS, CONTAIN UV STABILIZER AND LONG TERM..
Flexural Yield Strength 72.6 MPa
10500 psi
15 mm/min. ASTM D790
Techno Polymer Techno ABS LM100 Transparent
Excellent shock resistance, rigidity, and processability.Applications: Appliance parts, office and computer equipment, machine parts, and tool handles.
Flexural Yield Strength 72.6 MPa
10500 psi
ASTM D790
Samyang Trimma® SD6350H PMMA, Opaque
High scratch resistance; stability against weak acids, strong acids, weak alkalis and inorganic salts.Applications: Laptop, Monitor Front Cover - for high flow, high gloss and high hardnessInformat..
Flexural Yield Strength 72.6 MPa

@Thickness 3.20 mm
10500 psi

@Thickness 0.126 in
15 mm/min; ASTM D790
LG Chemical HF350U ABS, High Flow
Feature: Injection Molding, High Flow, Good WeatherabilityApplication: E & E Products (Monitor) )CAS No. 9003-56-9Information provided by LG Chemical