Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 53.8 MPa | 7800 psi | ASTM D790 |
Multibase Multi-Pro® 1508 M Polypropylene Mica Filled, 15% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase |
|||
Flexural Yield Strength | 53.8 MPa | 7800 psi | ASTM D790 |
Spartech Royalite R24 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 53.8 MPa | 7800 psi | ASTM D790 |
Spartech Royalite R57 FR/ABS Aircraft Grade Sheet Description: Aircraft Grade SheetInformation provided by Spartech. |