Polymer Property : Flexural Yield Strength = 827 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 5.70 MPa

@Strain 3.5 %
827 psi

@Strain 3.5 %
ISO 178
FKuR Kunststoff Terralene® LL 1303 Biobased Polyethylene
With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol..