Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 57.9 MPa @Thickness 3.20 mm |
8390 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical HI100 ABS, High Impact Feature: Injection Molding, High ImpactApplication: Helmet, Pipe & Fittings, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 57.9 MPa | 8390 psi | DIN 53455; ASTM D790 |
Kolon KOLEFIN® KO133MT30 M/F Reinforced Polypropylene KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica.. |
|||
Flexural Yield Strength | 57.9 MPa @Thickness 6.40 mm |
8390 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron HI-40 ABS High Impact Injection Molding Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali |
|||
Flexural Yield Strength | 57.9 MPa @Thickness 6.40 mm |
8390 psi @Thickness 0.252 in |
ASTM D790 |
Bhansali Engineering Abstron HI-40 B ABS High Impact Injection Molding Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali |
|||
Flexural Yield Strength | 57.9 MPa @Thickness 6.40 mm |
8390 psi @Thickness 0.252 in |
ASTM D790 |
Bhansali Engineering Abstron SE-22 FR Flame Retardant ABS Grade Information provided by Bhansali |
|||
Flexural Yield Strength | 57.9 MPa @Thickness 6.40 mm |
8390 psi @Thickness 0.252 in |
ASTM D790 |
Bhansali Engineering Abstron SE-22 FR Flame Retardant ABS Grade Information provided by Bhansali |
|||
Flexural Yield Strength | 57.9 MPa @Thickness 6.40 mm |
8390 psi @Thickness 0.252 in |
ASTM D790 |
Bhansali Engineering Abstron HI-40 B ABS High Impact Injection Molding Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali |
|||
Flexural Yield Strength | 57.9 MPa @Thickness 6.40 mm |
8390 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron HI-40 ABS High Impact Injection Molding Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali |
|||
Flexural Yield Strength | 57.9 MPa @Thickness 3.20 mm |
8390 psi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical HIPS MI750 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |