Flexural Yield Strength 175 - 840 MPa
25400 - 122000 psi
Average value: 310 MPa Grade Count:127
Overview of materials for Nylon 6, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E..