Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 928 MPa @Temperature 23.0 °C |
135000 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-3A Curing Cyanate Resin, M55J Fiber Information provided by HexCel |