Mechanical Properties Metric English Comments
Flexural Yield Strength 6.86 MPa
996 psi
ASTM D790
Samyang Triel® 5501BM Thermoplastics Polyetherester Elastomer, Blow Molding
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5501BM is for blow molding applications.Applications: Automotive BellowsInformation provided by Samyang...