Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 41.3685 - 999.74 MPa @Temperature 65.6 - 177 °C |
6000.01 - 145000 psi @Temperature 150 - 350 °F |
Average value: 301 MPa Grade Count:2 |
Overview of materials for Epoxy Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat.. |