Polymer Property : 1% Secant Modulus, MD = 190 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, MD 190 MPa
27600 psi
ISO 527-3
Polimeri Europa Clearflex® FG 306 Hexene Copolymer Linear Low Density Polyethylene
Clearflex FG 306 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, antiblocking and processing aid, suitable for blown film extrusion.Films manufactured with Clearf..
1% Secant Modulus, MD 190 MPa
27600 psi
ISO 527-3
Polimeri Europa Riblene® FM 34 Low Density Polyethylene - Blown Film Extrusion
Riblene FM 34 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 is characterized by a good balance between processabilit..
1% Secant Modulus, MD 190 MPa
27600 psi
ISO 527-3
Polimeri Europa Riblene® FM 34 E Low Density Polyethylene - Blown Film Extrusion
Riblene FM 34 E is a low density polyethylene (LDPE) with added slip (erucamide) and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 E is characterized by a good balance betwe..
1% Secant Modulus, MD 190 MPa
27600 psi
ASTM D882
SABIC HP0322N Low Density Polyethylene for Blown Film
Product Description: HP0322N is a Low Density Polyethylene grade suitable for producing heavy duty films and contains no slip or antiblock additives. It yields outstanding toughness and optical pr..