Polymer Property : 1% Secant Modulus, MD = 100 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, MD 100 MPa
14500 psi
ASTM D882
NOVA Chemicals Surpass® FPs317-A Octene sLLDPE Film Resin
Features: Exceptional puncture resistanceVery good tear propertiesLow gel levelExcellent optical properties Excellent elongation characteristics Easy to process, no drying required Applications: Cas..