Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, MD 135 MPa
19600 psi
ASTM D882
SABIC 318B Linear Low Density Polyethylene for Cast Film
Product Description: 318B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u..