Mechanical Properties Metric English Comments
1% Secant Modulus, MD 128 MPa
18500 psi
ASTM D882
ExxonMobil LD 307.76 Clear, High Impact Film Resin
LD 307.76 film has superior impact strength and heat sealability, used in frozen and other food packaging, and high strength bags.Information provided by ExxonMobil Chemical