Polymer Property : 1% Secant Modulus, MD = 19580 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, MD 135.0 MPa
19580 psi
ASTM D882
NOVA Chemicals Surpass® HPs900-C Octene sLLDPE Film Resin
Features: Easy processabilityExceptional clarity and glossLow gelExcellent seal properties Applications: High clarity applications Lamination film Coextruded sealant layerHigh toughness filmInformat..