Polymer Property : 1% Secant Modulus, MD = 202 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, MD 202 MPa
29300 psi
ASTM D882
ExxonMobil Exceed™ 1327CA Blown Film Resin  (discontinued **)
Exceed 1327CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1327CA resin have outstanding tensile, impact strength and puncture. These superi..