Mechanical Properties Metric English Comments
1% Secant Modulus, MD 166.7 MPa
24180 psi
ASTM D882
Lotte Chemical Titan TITANEX® LF1041 Linear low density polyethylene resin  (discontinued **)
LF1041 is a pelleted linear low density polyethylene resin formulated with antioxidant, high antiblock and slip agent. This product is used for blown film extrusion which offers outstanding toughne..
1% Secant Modulus, MD 166.7 MPa
24180 psi
ASTM D882
Lotte Chemical Titan TITANEX® LF1043 Linear low density polyethylene resin  (discontinued **)
LF1043 is a pelleted linear low density polyethylene resin formulated with antioxidant, and antiblock agent. This product is used for blown film extrusion which offers outstanding toughness, extrud..
1% Secant Modulus, MD 166.7 MPa
24180 psi
ASTM D882
Lotte Chemical Titan TITANEX® LF1044 Linear low density polyethylene resin  (discontinued **)
LF1044 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding toughness, extrudability and draw down..
1% Secant Modulus, MD 166.7 MPa
24180 psi
ASTM D882
Lotte Chemical Titan TITANEX® LF2021 Linear low density polyethylene resin  (discontinued **)
LF2021 is a pelleted linear low density polyethylene resin formulated with antioxidant, high antiblock and slip agent. This product is used for blown and cast film extrusion which offers outstandin..
1% Secant Modulus, MD 166.7 MPa
24180 psi
ASTM D882
Lotte Chemical Titan TITANEX® LF2024 Linear low density polyethylene resin  (discontinued **)
LF2024 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown and cast film extrusion which offers outstanding toughness, extrudability and ..
1% Secant Modulus, MD 166.7 MPa
24180 psi
ASTM D882
Lotte Chemical Titan TITANEX® LF2824 Linear low density polyethylene resin  (discontinued **)
LF2824 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown and cast film extrusion which offers outstanding toughness, extrudability and ..