Polymer Property : 1% Secant Modulus, MD = 255 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, MD 255 MPa
37000 psi
ASTM D882
DuPont Surlyn® 1650SB
DuPont™ Surlyn® 1650SB is available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Slip and antiblock agents are added to ..
1% Secant Modulus, MD 255 MPa
37000 psi
ASTM D882
Westlake LF2010 Hexene Linear Low Density Polyethylene
Westlake LF2010 is a hexene LLDPE with increased stiffness suitable for heavy duty films and shipping sacks. This material contains process aid for improved ease of extrusion, and can be blended wit..