Mechanical Properties Metric English Comments
1% Secant Modulus, MD 19.3 MPa
2800 psi
ASTM D882
Westlake EF706 Low Density Polyethylene
Westlake EF706 is a high melt index LDPE resin suggested for thin gauge garment films and other films requiring excellent drawdown. The high melt index makes this material a good choice in compound..